Nano and microstructure fabrication
High-aspect-ratio silicon deep etching with a pattern width of 80 nm and a depth of 6380 nm was achieved using the Bosch process. This process enabled precise control over the shape while maintaining a sufficient selectivity with the resist mask.
This advanced etching capability is ideal for applications requiring nano- and micro-scaled structures.