Precise etching control

Square-shaped pillars with a width of 28 μm were successfully fabricated using the Bosch Process. The pillars maintain their square geometry from top to bottom, demonstrating precise etching control.

  • Pillar height: 450 μm
  • Profile angle: 89.9°