Scientific paper on transparent conductive oxide solar cell by Tokyo Institute of Technology
Optically-rough and physically-flat TCO substrates for superstrate-type thin-film solar cells: Sol-gel Zn1−xMgxO coating on reaction-ion etched glass substrates
Lei Meng and Shinsuke Miyajima
Department of Electrical and Electronic Engineering, School of Engineering, Tokyo Institute of Technology, 2-12-1-NE-17, Ookayama, Meguro-ku, Tokyo, Japan
Solar Energy Materials and Solar Cells 2017 172, pp 230-237
Optically-rough and physically-flat transparent conductive oxides (TCO) substrates were created on glass substrates to promote light absorption of solar cells. Al doped Zn1−xMgxO (AZMO) transparent conductive thin film was etched in CFx based plasma using Samco RIE etcher RIE-10NR. The effects of gas mixture composition on etch rate was investigated.
Samco offers multiple types of RIE etchers from tabletop to 450 mm for various applications (plasma etching, photoresist ashing and plasma treatment). For more information on Samco RIE etcher lineup, please visit the product page below.
RIE Etcher (from tabletop to 450 mm)