Scientific Paper on Miniature Fuel Cell Fabrication from Tokyo University of Science

Miniature Fuel Cell with Monolithically Fabricated Si Electrodes-Reduction of Pt Usage by Pd-Pt Catalyst

Takayuki Honjo, Taku Matsuzaka and Masanori Hayase
Tokyo University of Science, Noda, Chiba, Japan
Presented at Power MEMS 2010, Nov 30-Dec 3, Leuven, Belgium

Samco RIE Etcher was used for silicon plasma etching over Cu mask in fuel channel fabrication of miniature fuel cells.


For more details of our silicon etching technologies, please visit the process data pages below.