Bulk vertical micromachining of single-crystal sapphire using inductively coupled plasma etching for x-ray resonant cavities
P-C Chen1, P-T Lin1, D G Mikolas1, Y-W Tsai2, Y-L Wang1, C-C Fu1 and S-L Chang2
1 Institute of Nano Engineering and Microsystems, National Tsing-Hua University, No. 101, Kuang-fu Rd, Sec. II, Hsinchu 300, Taiwan
2 Department of Physics, National Tsing-Hua University, No. 101, Kuang-fu Rd, Sec. II, Hsinchu 300, Taiwan
J. Micromech. Microeng. (2015) 25 015016
Samco ICP Etching System was used for the recipe optimization of sapphire plasma etching in x-ray resonant cavity fabrication.
For our process capabilities of sapphire plasma etching, please visit the page below.
Sapphire Dry Etching Process (ICP-RIE)