Novel Nano-Device to Measure Voltage-Driven Membrane Transporter Activity

Rikiya Watanabe, Naoki Soga, and Hiroyuki Noji
Dept. of Appl. Chem., Univ. of Tokyo, Tokyo, Japan
IEEE TRANSACTIONS ON NANOTECHNOLOGY (2016) 15, NO. 1

SAMCO open-load Reactive Ion Etching Tool was used for patterning of carbon-fluorine hydrophobic polymer (CYTOP) by dry etching of the layer against photoresist.