Design and fabrication of high-performance diamond triple-gate field-effect transistors
Jiangwei Liu 1, Hirotaka Ohsato 2, Xi Wang 1, Meiyong Liao 3 & Yasuo Koide 4
1 International Center for Young Scientists, National Institute for Materials Science (NIMS), 1-1 Namiki, Tsukuba, Ibaraki 305-0044, Japan.
2 Nanofabrication Platform, NIMS, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047, Japan.
3 Optical and Electronic Materials Unit, NIMS, 1-1 Namiki, Tsukuba, Ibaraki 305-0044, Japan.
4 Research Network and Facility Services Division, NIMS, 1-2-1 Sengen, Tsukuba, Ibaraki, 305-0047, Japan.
Scientific Reports 6, Article number: 34757 (2016)
Diamond is considered to be a material for next-gene