Scientific Paper on ZnO UV-Ozone Treatment for ZnO-FET Fabrication from Chiba University
Physical Property Evaluation of ZnO Thin Film Fabricated by Low-Temperature Process for Flexible Transparent TFT
Khafe, Adie Bin Mohd1; Watanabe, Hiraku1; Yamauchi, Hiroshi1; Kuniyoshi, Shigekazu1; Iizuka, Masaaki2; Sakai, Masatoshi1; Kudo, Kazuhiro1
1 Graduate School of Engineering, Chiba University, 1-33 Yayoi-cho, Inage-ku, Chiba, 263-8522, Japan
2 Faculty of Education, Chiba University, 1-33 Yayoi-cho, Inage-ku, Chiba, 263-8522, Japan
Journal of Nanoscience and Nanotechnology, Volume 16, Number 4, April 2016, pp. 3168-3175(8)
Samco UV-Ozone cleaner, UV-1 was used for ultraviolet/ozone (UV-O3) assisted thermal treatments on wet processed zinc oxide field effect transistor (ZnO-FET) to improve drain current and mobility of the ZnO-based device. They found that UV-Ozone treatment eliminated carbon impurities in ZnO thin film and improved the performance of ZnO-FET.
Scientific Paper on ZnO Nanorods Functionalization from Linköping University, Sweden
The improved piezoelectric properties of ZnO nanorods with oxygen plasma treatment on the single layer graphene coated polymer substrate
Mushtaque Hussain, Mazhar Ali Abbasi, Zafar Hussain Ibupoto, Omer Nur and Magnus Willander
Physical Electronic & Nanotechnology division, Department of Science &Technology, Campus Norrköping, Linköping University, SE-60174 Norrköping, Sweden.
physica status solidi (a) Volume 211, Issue 2, pages 455–459, February 2014
ZnO nanorods were treated with an oxygen plasma using SAMCO Plasma Etching System (RIE etcher) to reduce the defect levels.