Category: UV-Ozone

10 Sep

Scientific Paper on SU-8 Microlens Fabrication for LEDs from National Taiwan University

Samco 2015 Customer, LEDs, Samco Customer Publication, SU-8, Surface Treatment, UV-Ozone

Improved Light Uniformity From Light-Emitting Diodes by Heterogeneous Microlenses and 3-D Printed Mold

Cheng-Han Chiang and Guo-Dung John Su
Graduate Institute of Photonics and Optoelectronics, National Taiwan University, Taipei 10617, Taiwan
IEEE JOURNAL OF SELECTED TOPICS IN QUANTUM ELECTRONICS (2015) 21, NO. 4

SAMCO UV-Ozone cleaner was used for wettability modulation of SU-8 microlens.

22 Jul

Scientific Paper on Surface Enhanced Raman spectroscopy Tape Fabrication from A*STAR

Samco 2015 Customer, Samco Customer Publication, Surface Treatment, UV-Ozone

Flexible, transparent and robust SERS tapes through a two-step block copolymer self-assembly process

Vignesh Suresh and Fung Ling Yap
Institute of Materials Research and Engineering (IMRE), Agency for Science, Technology, and Research (A*STAR), 3, Research Link, Singapore 117602
RSC Adv., 2015, 5, 61671-61677

Samco table-top UV-Ozone cleaner was used for removal of organic contaminants in sample preparation.

12 Mar

Scientific Paper on TiO2 Surface Photocatalysis Research Using UV-Ozone Treatment by Peking University

Samco 2015 Customer, Samco Customer Publication, Surface Treatment, TiO2, UV-Ozone

Methanol Adsorption on TiO2 Film Studied by Sum Frequency Generation Vibrational Spectroscopy

Ran-ran Fenga,b, An-an Liua,b, Shuo Liua,b, Jiao-jian Shia,b, Yi Liua,b and Ze-feng Rena,b
a International Center for Quantum Materials (ICQM) and School of Physics, Peking University, Beijing 100871, China
b Collaborative Innovation Center of Quantum Matter, Beijing 100871, China
Chin. J. Chem. Phys. 28, 11 (2015)

Samco UV-Ozone cleaner was used for surface cleaning of TiO2 thin film in sample preparation.
Peking University is a proud customer of Samco UV-Ozone system, UV-1.

16 Jan

Scientific Paper on Nanowire Solar Cell by Kyung Hee University Team

Samco 2015 Customer, Samco Customer Publication, SU-8, Surface Treatment, UV-Ozone

Doubling Absorption in Nanowire Solar Cells with Dielectric Shell Optical Antennas

Sun-Kyung Kim Xing Zhang David J. Hill Kyung-Deok Song§ Jin-Sung Park§ Hong-Gyu Park§ and James F. Cahoon
Department of Applied Physics, Kyung Hee University, Gyeonggi-do 446-701, Republic of Korea
Department of Chemistry, University of North Carolina at Chapel Hill, Chapel Hill, North Carolina 27599-3290, United States
§Department of Physics, Korea University, Seoul 136-701, Republic of Korea
Nano Lett. 2015, 15, 753−758

Samco UV-Ozone cleaner, UV-1 was used for SU-8 stripping in nanowire-based device fabrication.

19 Aug

Scientific Paper on Multi-channel PMMA Microfluidic Biosensor by King Mongkut’s University and Cornell University

Samco 2013 Customer, Samco Customer Publication, Surface Treatment, UV-Ozone

Multi-channel PMMA microfluidic biosensor with integrated IDUAs for electrochemical detection

Nongnoot Wongkaewa,b, Peng Heb, Vanessa Kurthb, Werasak Surareungchaia, and Antje J. Baeumnerb
aSchool of Bioresources and Technology, King Mongkut’s University of Technology Thonburi, Bangkhuntien, Bangkok 10150,Thailand bDepartment of Biological and Environmental Engineering, Cornell University, 202 Riley Robb Hall, Ithaca, NY 14853, USA
Anal Bioanal Chem. 2013 July ; 405(18): 5965–5974. doi:10.1007/s00216-013-7020-0.

Samco UV-Ozone Cleaner at Cornell University was used for oxidation of PMMA to generate carboxylic groups on the surface in microfluidic biosensor fabrication. Samco UV-Ozone cleaners are used for many R&D labs of polymer biosensor fabrication for bonding of polymer materials, such as PDMS, PMMA , COP & COC.

29 Jun

Scientific Paper on Transparent Microelectrode Fabrication from Cornell University Team

Samco 2012 Customer, Samco Customer Publication, Surface Treatment, UV-Ozone

Transparent Electrode Materials for Simultaneous Amperometric Detection of Exocytosis and Fluorescence Microscopy

Kassandra Kisler1, Brian N. Kim1, Xin Liu2, Khajak Berberian1, Qinghua Fang1, Cherian J. Mathai3, Shubhra Gangopadhyay3, Kevin D. Gillis2,4, and Manfred Lindau1
1 School of Applied and Engineering Physics, Cornell University, Ithaca, NY USA
2 Dalton Cardiovascular Research Center, University of Missouri, Columbia, MO USA
3 Department of Electrical and Computer Engineering, University of Missouri, Columbia, MO USA
4 Departments of Biological Engineering and Medical Pharmacology and Physiology, University of Missouri, Columbia, MO USA
J Biomater Nanobiotechnol. 2012 ; 3(2A): 243–253.

Samco UV-Ozone cleaner at Cornell University was used for photoresist descum in sample preparation.

Our UV-Ozone cleaners are equipped with stage heating and ozone generator, and they enable high-speed photoresist ashing & stripping. The processes can be applied for photoresist decsum application. For more information on our UV-Ozone cleaners, please visit the product page below.
UV-Ozone Cleaners (Table-top & Production Models)