Scientific Paper on Plasma Treatment of PEEK for Better Adhesion with TiO2 Coating from Chubu University
Apatite-forming PEEK with TiO2 surface layer coating
Takashi Kizuki, Tomiharu Matsushita and Tadashi Kokubo
Department of Biomedical Sciences, College of Life and Health Sciences, Chubu University, 1200 Matsumoto-cho, Kasugai, Aichi 487-8501, Japan
J Mater Sci: Mater Med (2015) 26:41
DOI 10.1007/s10856-014-5359-1
A method for Polyetheretherketone (PEEK) surface treatment was investigated to achieve better adhesion with TiO2 film coating for biomedical applications. Oxygen plasma treatment of PEEK using Samco system improved adhesion between the material surface and TiO2 due to increase of oxygen-containing chemical functional groups on the surface.