Hierarchically nanostructured boron-doped diamond electrode surface
Takeshi Kondoa, b, c, Keita Yajimaa, Tsuyoshi Katoa, Masahiro Okanod, Chiaki Terashimab, c, Tatsuo Aikawaa, Masanori Hayaseb, d, Makoto Yuasaa, b, c
a Department of Pure and Applied Chemistry, Faculty of Science and Technology, Tokyo University of Science, 2641 Yamazaki, Noda, Chiba 278-8510, Japan
b Research Institute for Science and Technology, Tokyo University of Science, 2641 Yamazaki, Noda, Chiba 278-8510, Japan
c ACT-C/JST, 4-1-8 Honcho, Kawaguchi, Saitama 333-0012, Japan
d Department of Mechanical Engineering, Faculty of Science and Technology, Tokyo University of Science, 2641 Yamazaki, Noda, Chiba 278-8510, Japan
Diamond and Related Materials (2016)
A boron-doped diamond (BDD) electrode with a large specific surface area was fabricated. The combination of thermal treatment and whisker formation by diamond plasma etching was employed for nano-texturing of diamond surfaces. Samco open-load Reactive Ion Etcher, RIE-10NR was used for diamond plasma etching process.
For more details of our diamond plasma etching technologies and capabilities, please visit the process data page below.